Foshan Zhelu supplies hot top round bar, horizontal round bar, horizontal square bar, slab billet and rectangular crystallizers, in high-purity graphite on an aluminum-alloy or pure-copper base, with water curtain cooling and seal loop sealing. We supply crystallizers with a rational design, precise structure, excellent performance, easy disassembly and cleaning, and a long service life; they can be adapted to a wide range of casting conditions to meet customer requirements.
1. Uniform cooling around the billet, with cooling intensity set to form a shell of adequate strength before the billet leaves the mold.
2. Easy demolding, producing billet with good surface quality.
3. Simple structure, convenient installation, with adequate strength, rigidity and impact resistance.
4. High-purity graphite working face for lubrication and heat control at the meniscus.
5. Water curtain cooling gives even heat extraction around the circumference.
6. Seal loop sealing keeps cooling water where it belongs.
Molten aluminum enters the top of the crystallizer and meets the cooled mold wall. A shell forms against the wall and thickens as the billet is drawn downward by the casting machine. Cooling water, applied as a water curtain, extracts heat through the mold body; by the time the billet exits the bottom, the shell is thick enough to contain the remaining liquid core.
Shell formation is governed by cooling intensity and by how evenly it is applied. Cooling must be strong enough to build a shell that will not break out, and even enough that the shell thickness is the same all round — uneven cooling is what causes billets to crack or distort as they leave the mold. Two further parameters are set at design: the shrinkage rate of the ingot, which differs by alloy and by size, and the height of the crystallizer, which sets how much cooling the billet gets before release.
The metal leaves as a solid shell with a liquid core. Surface quality and internal soundness at this stage carry straight through to extrusion, which is why mold condition and cooling water condition matter more than most operators expect.
| Feature | Technical data |
|---|---|
| Product type | Hot top round bar crystallizer / Horizontal round bar crystallizer / Horizontal square bar crystallizer / Slab billet crystallizer / Rectangular crystallizer |
| Base material | aluminum alloy / Red copper |
| Crystallizer material | High purity graphite |
| Water outlet | Water curtain type |
| Sealing | Seal loop |
| Customization | Available to customer requirements |
Selection starts with billet size and shape — round bar, square bar, slab, or rectangular. Two further decisions follow: base material (aluminum alloy or red copper, chosen on the required cooling rate and budget) and crystallizer height, which depends on the shrinkage rate of the specific alloy and size you cast. Tell us your billet dimensions, alloy and casting speed, and we will specify the mold.
1. Hot top billet casting for extrusion billet.
2. Horizontal casting of round and square bar.
3. Slab and rectangular billet casting.
4. Replacement molds for existing casting machines.